    CARC powder coating

    Doesn't the high heat stuff require heat treatment to fully cure? I think it needs to be heated to like 300 degrees a few times for 20 minutes with 30 minute cooling intermissions in between?
  2. 1993

    CARC powder coating

    So originally I was looking into CARC for my HMMWV, but the powder coating is specifically an idea I'm researching for some "tactical" aluminum folding chairs I've designed. they are for indoor outdoor use. The feel and durability of CARC is something that I've grown very fond of and it may...
  3. 1993

    CARC powder coating

    Does anyone know a source for CARC powder coating? There's someone locally here that does powder coating but I'm guessing I'd have to supply the powder... I know that sherwin williams sells standard CARC formulas. Thanks!