Laminate vs. Basic vs. Supplemental Armor Windsheild Glass

Gunny456

New member
5
0
0
Location
Harper, Texas
The HMMWV parts manual list the above three windshield glass. Does anyone know the actual thickness of each of these? I have heard that the Basic Armor is 3/8" thick, but was is the listed laminate and supplemental armor glass thickness? Is there a source to purchase these glass?
 

86humv

Well-known member
Steel Soldiers Supporter
1,700
501
113
Location
Texas
Thin is about 3/8th...... .350 "
Thick is 5/8th.
Same as side glass.
All have the plastic on the inside.
 
Last edited:

suzukovich

Active member
389
141
43
Location
Gibsonton Fl
The stock windshield glass in mine has the DOT safety glass markings. That is already laminated. The armored glass is thicker and can be retrofitted to a standard M998.

Sent from my SM-J727U using Tapatalk
 
Top
AdBlock Detected

We get it, advertisements are annoying!

Sure, ad-blocking software does a great job at blocking ads, but it also blocks useful features of our website like our supporting vendors. Their ads help keep Steel Soldiers going. Please consider disabling your ad blockers for the site. Thanks!

I've Disabled AdBlock
No Thanks